Hot plonje plak asye galvanisedyo kouvwi ak yon kouch zenk metalik sou sifas la yo anpeche korozyon sou sifas la nan panno yo asye ak pwolonje lavi sèvis yo. Sa a se panèl asye zenk-kouvwi yo rele yon panèl galvanised.
Cho tranpeFèy asye galvanised. Yon plak asye mens benyen nan yon beny zenk fonn pou ke yon kouch zenk suiv sifas li yo. Li se sitou ki te pwodwi pa pwosesis la kontinyèl galvanize, se sa ki, plak yo asye woule yo kontinyèlman benyen nan yon beny plating ki gen zenk fonn fè plak asye galvanised;
Kondisyon sifas: Akòz metòd tretman diferan nan pwosesis la kouch, kondisyon yo sifas nan fèy papye galvanised yo tou diferan, tankou flè zenk òdinè, flè zenk amann, plat flè zenk, pa gen flè zenk, ak sifas fosfat. Estanda Alman tou presize nivo sifas yo.




Estanda teknik | EN10147, EN10142, DIN 17162, JIS G3302, ASTM A653 |
Klas asye | DX51D, DX52D, DX53D, DX54D, S220GD, S250GD, S280GD, S350GD, S350GD, S550GD; SGCC, SGHC, SGCH, SGH340, SGH400, SGH440, SGH490, SGH540, SGCD1, SGCD2, SGCD3, SGC340, SGC340, SGC490, SGC570; SQ CR22 (230), SQ CR22 (255), SQ CR40 (275), SQ CR50 (340), SQ CR80 (550), CQ, FS, DDS, EDDS, SQ CR33 (230), SQ CR37 (255), SQCR40 (275), SQ CR50 (340), SQ CR80 (550); oswa kliyan an Ekzijans |
Epesè | Kondisyon Kliyan an |
Lajè | Dapre egzijans Kliyan an |
Kalite kouch | Hot tranpe l 'asye galvanised (HDGI) |
Kouch zenk | 30-275g/m2 |
Tretman sifas | Pasivasyon (c), lwil (O), LACQUER sele (L), fosfat (P), trete (U) |
Estrikti sifas yo | Nòmal kouch Spangle (NS), minimize kouch Spangle (MS), Spangle-gratis (FS) |
Kalite | Apwouve pa SGS, ISO |
ID | 508mm/610mm |
Pwa bobin | 3-20 tòn metrik pou chak bobin |
Pakèt | Papye prèv dlo a se anbalaj enteryè, asye galvanised oswa kouvwi fèy asye se anbalaj deyò, plak gad palè bò, Lè sa a, vlope pa Sèt Steel Belt.or dapre kondisyon kliyan an |
Ekspòtasyon mache | Ewòp, Afrik, Azi Santral, Azi Sidès, Mwayen Oryan, Amerik di Sid, Amerik di Nò, elatriye |
Kalib epesè tab konparezon | ||||
Aparèy mesi | Dous | Aliminiòm | Galvanize | Prn |
Kalib 3 | 6.08mm | 5.83mm | 6.35mm | |
Kalib 4 | 5.7mm | 5.19mm | 5.95mm | |
Kalib 5 | 5.32mm | 4.62mm | 5.55mm | |
Kalib 6 | 4.94mm | 4.11mm | 5.16mm | |
Kalib 7 | 4.56mm | 3.67mm | 4.76mm | |
Kalib 8 | 4.18mm | 3.26mm | 4.27mm | 4.19mm |
Kalib 9 | 3.8mm | 2.91mm | 3.89mm | 3.97mm |
Kalib 10 | 3.42mm | 2.59mm | 3.51mm | 3.57mm |
Kalib 11 | 3.04mm | 2.3mm | 3.13mm | 3.18mm |
Kalib 12 | 2.66mm | 2.05mm | 2.75mm | 2.78mm |
Kalib 13 | 2.28mm | 1.83mm | 2.37mm | 2.38mm |
Kalib 14 | 1.9mm | 1.63mm | 1.99mm | 1.98mm |
Kalib 15 | 1.71mm | 1.45mm | 1.8mm | 1.78mm |
Kalib 16 | 1.52mm | 1.29mm | 1.61mm | 1.59mm |
Kalib 17 | 1.36mm | 1.15mm | 1.46mm | 1.43mm |
Kalib 18 | 1.21mm | 1.02mm | 1.31mm | 1.27mm |
Kalib 19 | 1.06mm | 0.91mm | 1.16mm | 1.11mm |
Kalib 20 | 0.91mm | 0.81mm | 1.00mm | 0.95mm |
Kalib 21 | 0.83mm | 0.72mm | 0.93mm | 0.87mm |
Kalib 22 | 0.76mm | 0.64mm | 085mm | 0.79mm |
Kalib 23 | 0.68mm | 0.57mm | 0.78mm | 1.48mm |
Kalib 24 | 0.6mm | 0.51mm | 0.70mm | 0.64mm |
Kalib 25 | 0.53mm | 0.45mm | 0.63mm | 0.56mm |
Kalib 26 | 0.46mm | 0.4mm | 0.69mm | 0.47mm |
Kalib 27 | 0.41mm | 0.36mm | 0.51mm | 0.44mm |
Kalib 28 | 0.38mm | 0.32mm | 0.47mm | 0.40mm |
Kalib 29 | 0.34mm | 0.29mm | 0.44mm | 0.36mm |
Kalib 30 | 0.30mm | 0.25mm | 0.40mm | 0.32mm |
Kalib 31 | 0.26mm | 0.23mm | 0.36mm | 0.28mm |
Kalib 32 | 0.24mm | 0.20mm | 0.34mm | 0.26mm |
Kalib 33 | 0.22mm | 0.18mm | 0.24mm | |
Kalib 34 | 0.20mm | 0.16mm | 0.22mm |











1. Ki pri ou ye?
Pri nou yo sijè a chanje depann sou ekipman pou ak lòt faktè mache. Nou pral voye ba ou yon lis pri ki ajou apre kontak konpayi ou
nou pou plis enfòmasyon.
2. Èske ou gen yon kantite lòd minimòm?
Wi, nou mande pou tout lòd entènasyonal yo gen yon kantite kontinyèl lòd minimòm. Si ou ap chèche revann men nan anpil pi piti kantite, nou rekòmande ou tcheke sit entènèt nou an
3. Èske ou ka bay dokiman ki enpòtan yo?
Wi, nou ka bay pifò dokiman ki gen ladan sètifika analiz / konfòmite; Asirans; Orijin, ak lòt dokiman ekspòtasyon kote sa nesesè.
4. Ki sa ki tan an plon mwayèn?
Pou echantiyon yo, tan an plon se sou 7 jou. Pou pwodiksyon an mas, tan an plon se 5-20 jou apre li fin resevwa peman an depo. Fwa yo plon vin efikas lè
(1) Nou te resevwa depo ou a, epi (2) nou gen apwobasyon final ou pou pwodwi ou yo. Si fwa plon nou yo pa travay ak dat limit ou, tanpri ale sou kondisyon ou yo ak vant ou. Nan tout ka nou pral eseye akomode bezwen ou yo. Nan pifò ka yo nou kapab fè sa.
5. Ki kalite metòd peman ou aksepte?
30% davans pa T/T, 70% pral anvan Shippment Debaz sou FOB; 30% davans pa T/T, 70% kont kopi a nan BL Basic sou CIF.